The purpose of this study was to investigate fracture strength of different lithium disilicate occlusal veneers designs
with different tooth preparations. Material and method: Fifty-six extracted human mandibular molars were collected
with relatively comparable size and standardization done by diamond saw and it will receive. 6mm lithium disilicate
occlusal veneers. Specimens will be divided into two main groups, each of these groups contains 28 samples (group
A&B), the first group represents occlusal veneers with 1.0 ml with radial shoulder finish line design includes axial
surfaces for a2 ml length, while the second group represents occlusal veneers preparation without finish line
Keywords
Occlusal Veneers, Lithium Disilicate, Additive Manufacturing.
Copyright
Copyright © Neuroquantology
Creative Commons License
This work is licensed under a Creative Commons Attribution-NonCommercial-NoDerivatives 4.0 International License.
Articles published in the Neuroquantology are available under Creative Commons Attribution Non-Commercial No Derivatives Licence (CC BY-NC-ND 4.0). Authors retain copyright in their work and grant IJECSE right of first publication under CC BY-NC-ND 4.0. Users have the right to read, download, copy, distribute, print, search, or link to the full texts of articles in this journal, and to use them for any other lawful purpose.